What is the Chinese equivalent of S235JR steel?

Jul 25, 2025 伝言を残す

What is the ASTM equivalent of S235?
ASTM A36,Q235B
EN 10025 S235JR ASTM equivalent steel grades are ASTM A36, ASTM A283 Grade C/A283 Gr.

 

What material is equivalent to ASTM A36?
The ASTM A36 plate is equivalent to grades like Q235B,ASTM A283C, JIS G3101 SS400, JIS G3106 SM400A, EN10025-2 S235JR, DIN17100 ST37-2, and FE360B.

 

What is the difference between S235 and S355 steel?
The primary difference between S235 and S355 steel lies in their yield strength. S355 has a higher minimum yield strength (355 MPa) than S235 (235 MPa), making it a stronger steel. While their chemical compositions are similar, S355's superior strength is achieved through specific rolling and cooling techniques during manufacturing.

 

What is S235 steel used for?

Each of these properties mean that S235 steel can be applied as structural components. Examples of where this steel is used include bridges and buildings. It's also utilised in military vehicles that need defending against explosive devices.

 

Is S235 steel magnetic?

Low-carbon steel (S235, C15) was specified as one of the primary products for magnetic coding because of its frequent use in industrial production

 

What is the equivalent of S235 steel?
Q235B
S235 steel, according to EN 10025, has several equivalent grades in other standards. The most common equivalents include GB Q235B,ASTM A36, JIS SS400, and DIN ST37-2.

A36 steel

 

What is the Chinese equivalent of S235JR steel?
Q235B
The closest Chinese equivalent to S235JR (EN 10025-2) is Q235B (GB/T 700-2006). While these grades share similar mechanical properties, subtle differences in composition and performance must be carefully evaluated for compliance and safety.